Observation of Vickers Indentation Made with Ultra Micro Hardness Tester

    Observation of Vickers Indentation Made with Ultra Micro Hardness Tester

    Microscopic indentations made with low loads that would be very difficult to measure with conventional methods can be observed clearly. Reverse image (right) gives a clear view of the deformation in the specimen at the tip of the indentation.